Resin bound driveways
A resin bound driveway is a mix of stone and resin spread over a tarmac or concrete base. Resin bonded is a different product, with stone scattered onto a coat of resin.
Checked against the sources on

In short
- Resin bound goes on a sound tarmac or concrete base. A British supplier says not to lay it over block paving.
- It only lets water through if the base underneath does too.
- Resin bonded does not let water through.
- Ask whether the resin is UV-stable. One maker says the other kind yellows over time.
The sources here are British manufacturers, suppliers and one magazine.
Resin bound and resin bonded
The two names are easy to mix up. Resin Bonded Aggregates, a British supplier, describes resin bound as "a system of laying a hardwearing course of mixed resin onto a new or existing tarmac or concrete base." The stone and resin are mixed first and spread together.
Resin bonded is the other way round: the resin is spread across the base and the stone is scattered into it. The same supplier says of bonded surfaces that "water cannot pass through; this means a Resin Bonded system is not porous."
The base underneath
Resin Bonded Aggregates accepts tarmac, asphalt and concrete as bases. It rules out block paving, setts and flags, because "The number of cracks or lines below the surface would ultimately lead to cracks in the resin". It says existing cracks in a base have to be fixed with a cross-layer membrane.
The suppliers give different thicknesses for a new base.
| Base | Resin Bonded Aggregates | GCL Products |
|---|---|---|
| Tarmac (macadam) | 50 mm of 14 mm porous close-graded surface course | More than 50 mm |
| Concrete | 100 mm of C25 smooth brushed concrete | More than 80 mm |
For the resin layer itself, GCL Products, a British manufacturer, describes spreading the mix to an even 18 mm depth.
Drainage through the surface
Resin bound is porous, but only on a porous base. Resin Bonded Aggregates says the surface lets water through into the ground beneath, and that "Laying a resin bound system onto an impermeable base will not be SUDS compliant." SuDS means sustainable drainage systems, and the compliance it refers to is a British planning matter.
The Irish rule for front gardens asks for a surface that is permeable or lets rain soak into the ground once it reaches 25 square metres or over half the garden. It does not name materials. See the permeable paving rule. If permeability matters for your drive, ask what the base will be made of as well as the top layer.
Resin type, weather and curing
GCL Products sells two kinds of resin. It describes UV-stable resin (also called aliphatic) as a premium resin that is clear and resists daylight, and says the other kind "will slightly yellow over time with the effects of UV rays from daylight."
GCL's guide describes laying on a dry, mild, cloudy day with no threat of rain. It names around 12 to 18 degrees Celsius as a good temperature, and says its resins are "cured/tack-free after 6 hours (non-UV) or 8-10 hours (UV)." It warns that in cold weather UV-stable resin may not cure at all until the laid mix reaches 5 degrees. The guide did not give times before walking or driving on the surface.
Cleaning
Resin Bonded Aggregates gives these points in its care guide:
- Do not use a jet wash or pressure washer setting above 150 bar.
- Keep the nozzle at least 20 cm from the surface.
- Clear leaves, twigs and debris regularly so weeds have less chance to seed.
It says moss or algae on a resin bound drive is relatively easy to remove, and that the surfaces are designed to resist weed growth.
Wear and cracking
Homebuilding & Renovating, a British magazine, says of resin bound driveways that "they tend to deteriorate relatively quickly, especially under heavy use or if installed poorly." It calls resin bonded more prone to cracking, especially under heavy traffic. These are the magazine's views rather than test results.
Sources
- Resin Bonded Aggregates: resin bound vs resin bonded (British supplier)
- Resin Bonded Aggregates: what is SUDS compliance? (British supplier)
- Resin Bonded Aggregates: resin bound system bases (British supplier)
- Resin Bonded Aggregates: understanding resin bound bases (British supplier)
- Resin Bonded Aggregates: resin bound maintenance guide (British supplier)
- GCL Products: resin bound gravel installation guide (British manufacturer)
- Homebuilding & Renovating: garages and driveways material guide (British)
This page is general information taken from published guidance. Products differ, so follow the laying and care instructions for the one you buy.
Related guides
- Which driveway surfaceSix driveway surfaces compared on rainwater, repairs, upkeep and cars.
- Gravel drivewaysStone size and depth, what goes underneath and how to keep the gravel in place.
- Tarmac drivewaysThe layers in a tarmac driveway, the materials suppliers name and how it ages.
- Drainage for driveways and patiosFalls, channel drains and soakaways, and where the rainwater is allowed to go.