Tarmac or block paving
Block paving can be lifted and relaid a few blocks at a time. Tarmac is cut out and patched, and the patch usually shows.
Checked against the sources on
In short
- A damaged block can be lifted and replaced. Tarmac is cut out and patched.
- Both come in permeable versions for front gardens that need one.
- Block joints need topping up with sand and weeding. Tarmac needs kerbs on every free edge.
- Permeable block paving should not be steeper than about 1 in 20.
- Most published comparisons come from block paving manufacturers.
Side by side
The table sets out what manufacturers, a trade body and a technical site say about each surface. Several of the sources are British.
| Block paving (cobblelock) | Tarmac | |
|---|---|---|
| Repairs | Blocks lifted out and replaced (Paving Expert, Tobermore) | Cut out and patched, and the patch usually shows (Paving Expert) |
| Drainage | Permeable blocks with stone-filled joints (Interpave, Tobermore, Roadstone) | Permeable asphalt sold (Holcim UK) |
| Slopes | Permeable paving no steeper than about 1 in 20 (Interpave, Tobermore) | No source found |
| Edges | Concrete kerbs set in concrete (Roadstone) | Edging or kerb on every free edge, or it crumbles (Paving Expert) |
| Weeds | Pull them as they appear, top up joint sand (Roadstone) | Can grow at the edges, beside lawns and beds (Aggregate Industries) |
| Upkeep | Clean two to three times a year, no pressure washer (Tobermore) | Clean up oil and fuel drips, care in hot weather while new (Aggregate Industries) |
| Look | Some colour variation is normal, white bloom on new blocks fades (Roadstone) | Black, fading to dark grey within 6 months to a year (Aggregate Industries) |
| Laying time | Marshalls says block paving can take longer to lay than tarmac. | |
Repairs
Paving Expert, a British technical site, says tarmac, bitmac and concrete can only be cut out and patched, usually leaving a visible reminder of the repair. A block surface can be opened up by taking out the blocks and relaid with the same ones. Tobermore, a Northern Ireland manufacturer, makes the same point, though its article is about roads rather than driveways. See cobblelock and block paving.
The Aggregate Industries aftercare leaflet adds that dents in tarmac can generally only be removed by patching. It says the risk of tyre damage to new tarmac is greatest when steering a car that is not moving, and higher in summer. See tarmac driveways.
Drainage and the front garden rule
A large paved area in a front garden has to be permeable, or drain to ground, to stay exempt from planning permission. See the permeable paving rule. Permeable block paving is made by Roadstone, Tobermore and others, with wider joints filled with grit instead of sand. Holcim UK sells a permeable asphalt that lets water through to a drainage layer below.
Tobermore says permeable blocks only suit ground that drains, and asks for a test hole for every 20 to 25 square metres of driveway. Both Interpave and Tobermore limit the slope to about 1 in 20. For steep driveways, Marshalls asks owners with "an incline of 15° or more" to contact its technical team.
Upkeep
Block paving needs its joints kept full. Roadstone says to top up the jointing sand 28 days after laying, and warns that mechanical sweepers can pull the sand out and cause "the loss of interlock and failure of the paved surface." Tarmac has no joints, but oil and fuel soften it, and the leaflet says oil dripping from a car can leave soft spots that break the asphalt down if they are not treated.
Marshalls, which makes block paving, says block paving is fairly easy to repair and that tarmac offers fewer choices in how it looks.
Sources
- Paving Expert: repairing and replacing paving (British)
- Paving Expert: laying bitmac and asphalt (British)
- Tobermore: How interlocking paving compares to asphalt for roads and adopted roads
- Tobermore: Guidelines for installing Hydropave permeable paving for domestic applications
- Marshalls: Block paving vs tarmac (British)
- Marshalls: Drivesys Driveway Concrete System Installation Guide, January 2020 (British)
- Interpave: Understanding Permeable Paving, Edition 5, April 2013 (British)
- Roadstone: Paving Laying & Maintenance Guide
- Roadstone: Ultracolour Colour Asphalt & Surface Treatments
- Aggregate Industries (Holcim UK): Asphalt Care, new asphalt surfaces, domestic and light use, January 2023 (British)
- Holcim UK: Asphalt for domestic projects (British)
This page is general information taken from published guidance. Products differ, so follow the laying and care instructions for the one you buy.
Related guides
- Cobblelock and block pavingBlock sizes and thicknesses, the layers underneath, laying patterns and the usual problems.
- Tarmac drivewaysThe layers in a tarmac driveway, the materials suppliers name and how it ages.
- Which driveway surfaceSix driveway surfaces compared on rainwater, repairs, upkeep and cars.
- Drainage for driveways and patiosFalls, channel drains and soakaways, and where the rainwater is allowed to go.